Good arc restriking even with cold wire tip, suitable for robot applications. Ideal for use in the field short arc and spray arc. Excellent gap bridging for root welding. High-efficiency type for economic production enviroments and CrMo-steels up to 550 °C (1022°F) . Due to the seamless production process the hydrogen content is below 3ml/100gr weld metal even after long storage in unconditioned condition.
Materials Boiler steels Cast steels - |
DIN 13CrMo44, 24CrMo5 GS 17CrMo55, GS 22CrMo54 |
EN 13CrMo4-5 G17CrMo5-5 G22CrMo5-4 |
ASTM Typical A 387 Gr. 11-12 |
similarly alloyed heat treatable steels.
similarly alloyed cementation and nitrided steels.