CEWELD


9015-B9 SMAW Stick Electrodes




9015-B9

 
TYPE 
Basic, Cr and Mo-alloyed electrode for heat resistant steels T/P91 and T/P92
APPLICATIONS 
Headers, main steam piping and turbine casings, in fossil fuelled power generating plants. Oil refineries and coal liquefaction and gasification plants. Preheat and Interpas temperature 200°C - 300°C.
PROPERTIES 

9015-B9 is designed to weld equivalent ‘type T91’ T92 CrMo steels modified with small additions of vanadium and tungsten to give improved long term creep properties. These consumables are specifically intended for high integrity structural service at elevated temperature so the minor alloy additions responsible for its creep strength are kept above the minimum considered necessary to ensure satisfactory performance. In this case, weldments will be weakest in the softened (intercritical) HAZ region of parent material, as indicated by so-called ‘type IV’ failure in transverse weld creep tests.

CLASSIFICATION
AWS 
A 5.5: E 9015-B9
EN ISO 
3580-A: E CrMo91 B 42 H5
SUITABLE FOR 

X11CrMo9-1, X12CrMo9.1, X20CrMoV10-1, 1.7389, 1.7386, 1.4922, 1.4935, 1.4904 ASTM: A 199Gr.T9, A335Gr. P9, A351, A213/213M, P91, P92

APPROVALS 
CE approved
WELDING POSITIONS: 
ANALYSES %

C

Mn

Si

Cr

Ni

Mo

V

N

Nb

 

0.1

0.8

0.35

9.0

0.7

1.0

0.2

0.04

0.05

 

PWHT: 750°C/2hr, oven cooling till 300°C and then cooled on air.

MECHANICAL PROPERTIES

Heat

RP0,2

Rm

A5

Impact Energy (J) ISO-V

Hardness

Treatment

(N/mm2)

(N/mm2)

(%)

+20°C

-40°C

-60°C

HRc / HV

AW

>650

760

>17

>70 J

     
AW = as welded
REDRYING TEMPERATURE 
350°C/1hr
WELDING PARAMETERS / PACKING

Welding Parameters

Packing

D (mm)

Length (mm)

Current (A)

kg / can

kg / 6pack

kg / 1000

2.5

350

70-110

2.4

14.4

19.8

3.2

350

95-150

2.4

14.4

36.4

4.0

350450

130-190

3.0

18

66.7