The weld deposit is scale-resistant up to approx. 800°C in normal atmosphere and oxidizing gases. The weld deposit is capable of taking a high polish
1.4306 1.4301 1.4541 1.4550 1.4552 1.4312 1.4546 1.4311 |
X2CrNi 19 11 |
(TP) 304L (TP) 304 (TP) 321 (TP) 347 CF-8C, 302 (TP) 302 - |
.
⇒1.4303, 1.4308, 1.4310, 1.4312, 1.4319