Mn, Ni, Cr and Mo alloyed basic electrode for welding low alloyed steels with tensile strength >690 N/mm2. Crack resistant and well suited for low-temperatures, ductility down to -60°C. Preheating, interpass temperature and post weld treatment as required for the base metal. Hydrogen content: < 3 ml / 100 g weld metal.
S620, S550, Hardox, S620Ql1, S600MC, Naxtra 63, TStE620, Weldox 500, Hardox, Domex 460 MC, Domex 500 MC, Domex 550 MC, Domex 600 MC, Domex 650 MC, L480 - L550, X65 - X80, Hardox 400, XAR 400, Dilidur 400, 20MnCr65, 28CrMn43