ApplicationCr-wire/rod for joining ferritic/martensitic Cr-steels/ cast steels and for surfacing un-/low alloyed steels/ high strength steels/cast steels. Corrosion resistant
as equivalent 13% Cr steels for service temperatures up to 450°C. Surfacing of gas valves and fittings.
Chemical CompositionC: 0,10 Si: 0,50 Mn: 0,60 Cr: 11,5-13,5 Mo:0,6
Element by weight (%)
Mechanical PropertiesYield Strength (Re)380 N/mm²
(Typical)Tensile Strength (Rm)550 N/mm²
Elongation (A)(Lo05do)15%
Hardness (HB30)35 HRC without heat treat.
180 HB (680°C/8h)
Approvals-
Shielding gas/PolarityWIG:(ISO 14175)I1(=-)
MSG: (ISO 14175)M12,M13(=+)
Typical Base Material1.4000 1.4001 1.4002 1.4003
1.4006 1.4008 1.4021 1.4024
PackagingMIG/MAG: spools D 100 / D 200 / K 200 / K 300