ApplicationStabilised CrNiNb-wire/rod for joining and surfacing corrosion resistant steels/cast steels for service temperatures from –110°C up to + 400°C.
Chemical CompositionC: 0,06 Si: 0,85 Mn: 1,30Cr: 19,50 Ni: 9,50
Element by weight (%)Nb: 12xC
Mechanical PropertiesYield Strength (Re)490 N/mm²
(typical)Tensile Strength (Rm)680 N/mm²
Elongation (A)(Lo=5do)32%
Impact energy (Av)80 J
High temp.400°C
Low temp.-110°C
ApprovalsTÜV, DB, -Zeichen
Shielding gas/PolarityWIG:(ISO 14175)I1(=-)
MSG: (ISO 14175)M12,M13(=+)
Typical Base Material1.43011.43061.45411.43101.3212
1.45501.45521.43191.4303
TUV Kennblatt 1000: Group 29
ISO 20172: Gruppe 8.1 (exept Mo)
PackagingMIG/MAG: spools D 100 / D 200 / K 200 / K 300 / C 300