CEWELD


SA Alloy 825 SAW Arc Submerged




SA Alloy 825

 
CATEGORY 
TYPE 
Nickel - Chromium - Molybdenium - Copper alloy for SAW welding.
APPLICATIONS 
The excellent corrosion-resistant properties of Alloy 825 make the alloy a suitable choice for a variety of difficult applications. Uses include fabricated equipment found in chemical and petro- chemical processing, pulp and paper manufacturing, flue gas desulphurization systems and metal pickling operations.
PROPERTIES 

Fully austenitic weld metal with high resistance against stress corrosion cracking and pitting in media containing chloride ions. Good corrosion resistance against reducing acids due to the combination of Ni, Mo and Cu. Sufficient resistance against oxidizing acids. The weld metal is corrosion resistant in sea water. SA Alloy 825 is best to be used with FL 839 flux.

CLASSIFICATION
AWS 
A 5.14: ER NiFeCr-1
UNS N08065
EN ISO 
18274: S Ni8065
(NiFe30Cr21Mo3)
DIN: W.Nr. 
2.4858
SUITABLE FOR 

G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, ALLOY 825, N08028, UNS N08825 W.Nr: 1.4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465, 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586

APPROVALS 
CE approved
WELDING POSITIONS: 
ALL-WELD METAL ANALYSES % (TYPICAL)

C

Mn

Si

Cr

Ni

Mo

Cu

Ti

Fe

<0.05

<0.1

<0.4

19.5-23.5

38-46

2.5-3.5

1.5-2.8

0.6-1.2

>22

MECHANICAL PROPERTIES (TYPICAL)

Flux type

RP0,2

Rm

A5

Impact Energy (J) ISO-V

Hardness

as welded

MPa

MPa

(%)

20°C

-40°C

-196°C

HRc / HV

FL 839

425

630

30

   

70

 
REDRYING TEMPERATURE 
not required
WELDING PARAMETERS / PACKING

Welding Parameters

D (mm)

Voltage (V)

Current (A)

Travel speed (cm/min)

1,6

26-29

225-325

35-60

2,4

29-33

300-400

35-60

3,2

29-33

350-500

35-60