Submerged arc welding wire to be used with FL 8111 or FL 880 flux with excelent welding properties. Stainless deposit with low carbon content. Low heat input is recommended to avoid pronounced grain coarsening. Absence of stabilisation means that this steel is distinctly vulnerable to sensitisation phenomenon during welding, even though martensite hogs a great amount of carbon and nitrogen.
Cladding AISI 410, 410NiMo, 410NiMoNbV.